Hygroscopic crystal resources deteriorate when they're not usually saved in sufficiently dry air (or a dry purge fuel). This applies e.g. to KDP and BBO, As well as in a lesser extent to LBO. It may be practical to keep this type of crystal in a considerably elevated temperature, that makes it easier to continue to keep it dry.If the crystal surfa